Most likely Douglas-fir; alternatives include western hemlock or reclaimed pine. — Pseudotsuga menziesii

Most likely Douglas-fir; alternatives include western hemlock or reclaimed pine.

Pseudotsuga menziesii · Softwood (conifer), apparently weathered/reclaimed.

AI-generated identification · may be incorrect
Type
Softwood (conifer), apparently weathered/reclaimed.
Origin
Western North America, especially the Pacific Northwest and inland western regions.
Hardness
Janka approximately 620 lbf — Soft.
Durability
Slightly durable; heartwood has limited decay resistance, while exposed weathering can produce surface degradation and insect damage.

Got a wood sample like this?

Identify any wood from a photo, free.

Identify wood

Grain Pattern

Predominantly straight, vertical grain with pronounced earlywood/latewood bands; surface appears flat-sawn and heavily weathered, with no clear decorative figure.

Color & Appearance

Originally likely pale pinkish-brown heartwood with lighter sapwood; ultraviolet exposure and abrasion have produced a gray-brown patina and low luster.

Hardness (Janka)

Janka approximately 620 lbf — Soft.

Durability & Decay Resistance

Slightly durable; heartwood has limited decay resistance, while exposed weathering can produce surface degradation and insect damage.

Value & Age

Estimated Market ValueNot an official valuation

Approximately $2–$6 per board foot for ordinary dry Douglas-fir; reclaimed or selected material may cost $5–$15+.

AI estimate for general guidance only — not a professional appraisal. Actual value depends on grade, dimensions, condition, and local market demand.

Wood Age Estimate
The board’s surface weathering suggests years to decades of exposure, but visual evidence cannot establish tree or board age.

Common Uses

Framing, beams, siding, decking, trim, furniture, flooring, and reclaimed architectural lumber.

Geographic Origin

Western North America, especially the Pacific Northwest and inland western regions.

Workability

Generally machines, planes, sands, glues, and fastens well; resin, uneven grain, and weathered fibers may cause tearout or blunt edges.

Finish Recommendations

Remove gray fibers by scraping or sanding, then use a penetrating exterior oil or stain; clear film finishes require thorough preparation and maintenance.

Notable Features

Strong growth-ring contrast, relatively light weight, and characteristic resinous conifer structure; visible checking and erosion indicate outdoor exposure.

Learn more about Most likely Douglas-fir; alternatives include western hemlock or reclaimed pine. in the Wood Encyclopedia
Identified September 14, 2026