Most likely red oak, possibly white oak or another oak-like hardwood; the image shows a mixed/assembled surface rather than one clearly identifiable board.
Quercus rubra (alternatives: Quercus alba or related Quercus species) · Hardwood; likely domestic oak flooring or reclaimed/used stock.
AI-generated identification · may be incorrect- Type
- Hardwood; likely domestic oak flooring or reclaimed/used stock.
- Origin
- Eastern and central North America; commonly grown and milled throughout the United States and Canada.
- Hardness
- About 1,290 lbf Janka for red oak—Hard; white oak is about 1,360 lbf.
- Durability
- Slightly to moderately durable; heartwood has useful rot resistance, but untreated oak is not ideal for prolonged exterior exposure.
Got a wood sample like this?
Identify any wood from a photo, free.
Grain Pattern
Mostly straight, open-grained growth with plain-sawn cathedral and occasional irregular streaking; no distinctive figured pattern is evident.
Color & Appearance
Muted tan to medium brown with darker gray-brown oxidation, sapwood-like pale strips, and visible wear. Oak typically deepens slightly amber-brown with age and light.
Hardness (Janka)
About 1,290 lbf Janka for red oak—Hard; white oak is about 1,360 lbf.
Durability & Decay Resistance
Slightly to moderately durable; heartwood has useful rot resistance, but untreated oak is not ideal for prolonged exterior exposure.
Value & Age
Approximately $4–$10 per board foot for ordinary kiln-dried oak; reclaimed or select material may differ substantially.
AI estimate for general guidance only — not a professional appraisal. Actual value depends on grade, dimensions, condition, and local market demand.
- Wood Age Estimate
- The surface appears worn and oxidized, suggesting years to decades of use, but sample age cannot be determined visually.
Common Uses
Flooring, furniture, cabinetry, trim, veneer, barrels, and general interior joinery.
Geographic Origin
Eastern and central North America; commonly grown and milled throughout the United States and Canada.
Workability
Machines and sands well, though open pores and occasional grain reversal can cause tear-out; predrilling improves fastening, and gluing is generally reliable.
Finish Recommendations
Clean and sand progressively, then use dewaxed shellac, oil, lacquer, or polyurethane; grain filler can produce a smoother finish.
Notable Features
Prominent open pores, moderate weight, and characteristic oak grain; the visible assembly may include boards of differing grades or species.