Likely oak (white oak group); exact species cannot be confirmed from this end-grain view. Possible alternatives include red oak or chestnut oak.
Quercus spp.; possibly Quercus alba or another North American oak. · Hardwood
AI-generated identification · may be incorrect- Type
- Hardwood
- Origin
- If North American oak, likely from eastern North America; oaks also grow widely across Europe and Asia.
- Hardness
- Oak varies by species: white oak about 1,360 lbf and northern red oak about 1,290 lbf—Hard.
- Durability
- White oak is Durable; red oak is Slightly Durable. Species identification is needed to judge rot and insect resistance reliably.
Got a wood sample like this?
Identify any wood from a photo, free.
Grain Pattern
Coarse, mostly straight grain with prominent growth rings; the log’s flat-sawn face may show cathedral figure. Bark and end-grain condition limit assessment of finer figure.
Color & Appearance
Freshly exposed wood is light to medium tan-brown, with darker growth-ring bands and possible oxidation; sapwood and heartwood are not clearly separable here.
Hardness (Janka)
Oak varies by species: white oak about 1,360 lbf and northern red oak about 1,290 lbf—Hard.
Durability & Decay Resistance
White oak is Durable; red oak is Slightly Durable. Species identification is needed to judge rot and insect resistance reliably.
Value & Age
Roughly US$5–12 per board foot for common kiln-dried oak lumber; a wet, ungraded log has no dependable equivalent price.
AI estimate for general guidance only — not a professional appraisal. Actual value depends on grade, dimensions, condition, and local market demand.
- Wood Age Estimate
- Not reliably estimable from the image; exposed end grain and bark do not establish the tree’s age or how long it has been cut.
Common Uses
Furniture, flooring, cabinetry, barrels, joinery, veneer, and construction; uses depend on species and grade.
Geographic Origin
If North American oak, likely from eastern North America; oaks also grow widely across Europe and Asia.
Workability
Generally machines and finishes well, though coarse grain can splinter or tear out; predrilling helps with fasteners.
Finish Recommendations
Sand progressively and apply oil, shellac, lacquer, or polyurethane; use a grain filler for a smoother, glass-like finish.
Notable Features
Oak has conspicuous growth rings and usually large pores; white-oak-group woods have tyloses that improve liquid resistance compared with red oak.