White Oak
Quercus alba · Hardwood
AI-generated identification · may be incorrect- Type
- Hardwood
- Origin
- Eastern North America
- Hardness
- 1350 lbf (Hard)
- Durability
- Very Durable with high resistance to decay and moisture.
Got a wood sample like this?
Identify any wood from a photo, free.
Grain Pattern
Straight grain with a medium to coarse texture and prominent growth rings.
Color & Appearance
Light to medium brown heartwood with a paler sapwood, darkening slightly with age and light exposure.
Hardness (Janka)
1350 lbf (Hard)
Durability & Decay Resistance
Very Durable with high resistance to decay and moisture.
Value & Age
4.00 to 8.00 USD per board foot
AI estimate for general guidance only — not a professional appraisal. Actual value depends on grade, dimensions, condition, and local market demand.
- Wood Age Estimate
- Mature standing tree bark, estimated at 50 to 100 years based on furrow depth.
Common Uses
Furniture, flooring, cabinetry, boat building, and tight cooperage.
Geographic Origin
Eastern North America
Workability
Goods results with hand and machine tools, though prone to staining from iron fasteners.
Finish Recommendations
Takes stains, oils, and polyurethane exceptionally well after proper sanding.
Notable Features
High tannin content and closed cellular structure providing natural water resistance.