White Oak
Quercus alba · Hardwood
AI-generated identification · may be incorrect- Type
- Hardwood
- Origin
- Eastern North America
- Hardness
- 1360 lbf (Hard)
- Durability
- Very Durable with high resistance to decay and moisture.
Got a wood sample like this?
Identify any wood from a photo, free.
Grain Pattern
Straight grain with a medium to coarse texture and prominent growth rings.
Color & Appearance
Light to medium brown heartwood with a paler sapwood, darkening slightly with age and light exposure.
Hardness (Janka)
1360 lbf (Hard)
Durability & Decay Resistance
Very Durable with high resistance to decay and moisture.
Value & Age
5.00 to 12.00 USD per board foot
AI estimate for general guidance only — not a professional appraisal. Actual value depends on grade, dimensions, condition, and local market demand.
- Wood Age Estimate
- Freshly cut or recently harvested round log.
Common Uses
Furniture, flooring, cabinetry, boat building, and exterior construction.
Geographic Origin
Eastern North America
Workability
Good overall workability, though it can react with iron and requires pre-boring for screws.
Finish Recommendations
Accepts stains, oils, and polyurethane finishes well with minimal preparation.
Notable Features
High tannin content and closed cellular structure providing natural water resistance.