White Oak
Quercus alba · Hardwood
AI-generated identification · may be incorrect- Type
- Hardwood
- Origin
- Eastern North America
- Hardness
- 1360 lbf (Hard)
- Durability
- Very Durable with high natural resistance to rot and decay.
Got a wood sample like this?
Identify any wood from a photo, free.
Grain Pattern
Straight, open grain with prominent growth rings and distinct medullary rays.
Color & Appearance
Light to medium brown heartwood with a paler sapwood, darkening slightly to an amber tone over time.
Hardness (Janka)
1360 lbf (Hard)
Durability & Decay Resistance
Very Durable with high natural resistance to rot and decay.
Value & Age
6 to 12 dollars per board foot
AI estimate for general guidance only — not a professional appraisal. Actual value depends on grade, dimensions, condition, and local market demand.
- Wood Age Estimate
- Estimated 20 to 50 years based on surface oxidation and seasoning checks.
Common Uses
Furniture, flooring, cabinetry, boat building, and barrel staves.
Geographic Origin
Eastern North America
Workability
Accepts screws, glue, and nails well, though pre-boring is recommended to prevent splitting.
Finish Recommendations
Takes oil, lacquer, and polyurethane finishes exceptionally well after proper sanding.
Notable Features
Contains high levels of tyloses which naturally block pores and prevent liquid penetration.