White Oak
Quercus alba · Hardwood
AI-generated identification · may be incorrect- Type
- Hardwood
- Origin
- Eastern North America
- Hardness
- 1360 lbf (Hard)
- Durability
- Very Durable, with high natural resistance to rot and fungal decay.
Got a wood sample like this?
Identify any wood from a photo, free.
Grain Pattern
Straight grain with prominent growth rings and distinct ray fleck patterns from quarter-sawing.
Color & Appearance
Light to medium brown heartwood with a paler sapwood, darkening slightly to an amber tone with age.
Hardness (Janka)
1360 lbf (Hard)
Durability & Decay Resistance
Very Durable, with high natural resistance to rot and fungal decay.
Value & Age
6 to 12 USD per board foot for standard lumber grades.
AI estimate for general guidance only — not a professional appraisal. Actual value depends on grade, dimensions, condition, and local market demand.
- Wood Age Estimate
- Estimated at 5 to 15 years, showing minimal oxidation and modern milled edges.
Common Uses
Furniture, flooring, cabinetry, boat building, and tight cooperage.
Geographic Origin
Eastern North America
Workability
Good overall workability, though it can react with iron and requires pre-boring for nails.
Finish Recommendations
Accepts stains, polyurethane, and oils well; requires no special primer.
Notable Features
Closed cellular structure due to tyloses, giving it excellent water resistance.